ION 41 there is of blurring, since the particles seem not to be of sufficient size to scatter the light. It should be noted, that in some collodion dry-plate processes, the preservative used has a tendency to cause halation, which is due, in a great measure, to the action of the preservative… … Fig. 19 Fig. 20. particles of liquid lying in the film scatter the light and give rise to halation ; but the emulsion processes are those which are most prone to show it in its worst form. An exact estimate of the amount of blurring that may be expected may be formed by cutting out in tinfoil a…